What is a heat number on a casting?
A heat number is the identity a foundry gives to one melt of metal: one furnace charge, melted, adjusted, analyzed and poured. Every casting and test bar poured from that melt carries the heat number, and the chemical analysis on the certificate belongs to it. The heat number is the anchor of the whole traceability chain.
Foundries mark the heat number on the casting, usually cast in with letters in the pattern or stamped after cleaning, together with a part number, pattern number and often a serial. If the marking is ground off during fettling or machining, it must be transferred before it is lost, and the transfer recorded.
Heat number vs cast number vs lot number: what is the difference?
Heat number and cast number usually mean the same thing: the melt identity. A lot number groups items that share a process step, most often a heat treatment load. A serial number identifies one piece. A data book for castings needs all of them to agree wherever they appear.
| Identity | What it identifies | Where it appears | What it links to |
|---|---|---|---|
| Heat number (cast number) | One melt | Casting marking, certificate, spectrometer printout, test bars | Chemistry, tensile and impact results |
| Heat treatment lot (load number) | One furnace load | Furnace chart, heat treatment certificate, certificate remarks | Mechanical properties after treatment |
| Test bar identity | The bar representing a heat, and sometimes a lot | Bar stamp, test report | Tensile, Charpy and hardness results |
| Serial number | One casting | Casting marking, NDT reports, dimensional report, hydro test | Per-piece tests and final inspection |
| PO line and part number | The ordered item | PO, certificate, cover | The contract |
One melt may fill several heat treatment loads, and one load may contain castings from several heats. That many-to-many relationship is where most traceability findings come from.
How does the traceability chain run from melt to data book?
The traceability chain for a casting runs from the melt through pouring, test bars, shakeout and marking, heat treatment, testing, NDT, machining and final inspection, ending in the certificate and the data book. Each step adds a record, and each record must carry the identity that connects it to the step before.
Text equivalent of the diagram
- Melt (heat number assigned) → spectrometer printout carries the heat number.
- Pour → castings and test bars carry the heat number.
- Shakeout, cleaning, marking → casting gets heat number, part number and serial.
- Heat treatment → castings and their test bars go into a furnace load; the furnace chart lists the load number and the heats and serials in it.
- Mechanical testing → test report carries the test bar identity, heat number and load number.
- NDT and repair → reports carry serial and heat; repair maps carry serial.
- Machining and pressure test → marking transferred if removed; reports carry serial.
- Certificate → heat number, load number, test results, quantity per PO line.
- Data book → every document above, in the buyer's index order, with identities matching.
How do test bars stay traceable?
Test bars stay traceable when each bar is marked with its heat number as it is poured, and with its heat treatment load when it goes into the furnace with the castings it represents. The test report must then carry the same identities. A test result that cannot be tied to a heat and load cannot represent any casting.
Separately cast bars and cast-on bars fail in different ways:
- Separately cast bars are poured into their own molds, such as keel blocks or Y-blocks. They are easy to lose track of because they are not attached to anything. Mark them at the mold, not after shakeout.
- Cast-on bars are attached to the casting and carry its identity until they are cut off. The risk comes at cutting: once removed, a cast-on bar needs its own marking before it leaves the casting.
The Steel Founders' Society of America notes that test bars should be heat treated in production furnaces with the castings they represent. A bar treated in a later load, even at the same settings, represents that later load, not the castings.
For low temperature ductile iron grades, record which kind of bar was used. EN 1563 distinguishes separately cast samples from cast-on samples in the grade designation itself (a "U" suffix for cast-on), so the bar type is part of what the certificate claims.
Why do heat treatment loads break traceability?
Heat treatment loads break traceability because they regroup castings. A load can hold castings from several heats, and one heat can be spread over several loads. If the furnace chart lists only the load number and not the heats and serials inside it, a reviewer cannot prove which castings had which treatment.
What a reviewer needs to see for each casting:
- The load number it was treated in.
- The furnace chart for that load, showing the cycle.
- A load list naming the heats and serials in the load.
- The test bars that represent the load, if properties are certified per load.
If any casting was re-heat-treated, the book needs both loads and a note explaining why. Re-treatment after a failed test is common and acceptable when it is documented; a second furnace chart with no explanation is a finding.
The heat number on the certificate does not match the casting. What now?
When the heat number on a certificate does not match the casting, stop and find out which record is wrong before changing anything. Most mismatches are transcription errors on one document. Some are real: a replacement casting from a different heat, or a marking error on the part. Each needs a different correction.
- Hold the book. Do not correct any document by hand.
- Check the marking on the casting itself, with a photograph.
- Check the melt log and the spectrometer printout for both heat numbers.
- Check the pouring record: which castings and bars were poured from each heat.
- Check whether the casting was a replacement from a later heat.
- If one document has a transcription error, have its issuer reissue it with a revision note.
- If the casting is from a different heat, include that heat's certificate and test results, or raise a concession with the buyer.
- If the marking on the part is wrong, follow your nonconformance procedure and the buyer's requirements for re-marking.
Never retype a certificate to make it match. Under EN 10204:2004, an intermediary may only pass on a manufacturer's inspection document without alteration, and a foundry that edits its own validated certificate after the fact creates a worse finding than the one it was fixing.
How is traceability different for forgings?
Forging traceability starts one step earlier: the forge usually buys ingot or bar from a steelmaker, so the heat number belongs to the steelmaker's melt and arrives on the steelmaker's certificate. The forge adds its own identities for the forging, heat treatment load and serial, and must keep the steelmaker's heat number on the forging.
For a forging book, check that:
- The steelmaker's certificate is included unchanged and its heat number matches the forging marking.
- The forge's certificate references the same heat.
- Test locations (from the forging, a prolongation or a separate test forging) are stated and tied to the heat treatment load.
- Per-piece UT reports carry the serial.
What this means for your data book
- Make sure every document carries the heat, load or serial that connects it to the step before.
- List heats, serials and test bars on every furnace load sheet.
- Mark separately cast bars at the mold, and cast-on bars before they are cut off.
- Record re-heat-treatment with both charts and a reason.
- Never correct a certificate by hand. Have it reissued.
How to check a data book, step by stepData book software for foundries and forges
Sources
Sources are listed in the order they are cited. Standards are cited by number and clause; consult your own licensed copy for their requirements.
- Steel Founders' Society of America, "Test Coupons and Casting Properties". www.sfsa.org/publications/testcoupons/tc.pdf
- ASTM International, A703/A703M "Steel Castings, General Requirements, for Pressure-Containing Parts" (abstract: coupons cast from the same heat as the castings; tension test per heat). store.astm.org/a0703_a0703m-07.html
- Applus+ Laboratories materials portal, EN-GJS-400-18U-LT datasheet (cast-on sample designation). www.appluslaboratories.com/materials-portal/datasheet/en-gjs-400-18u-lt-en-js1049/1463095379
- CEN, EN 10204:2004, clause 6 "Transmission of inspection documents by an intermediary" (consult your licensed copy). Publisher listing: shop.standards.ie/en-ie/standards/en-10204-2004-325038_saig_cen_cen_749388
- International Association of Drilling Contractors, "IADC Manufacturing Record Book Guidance" (traceability on every page). iadc.org/wp-content/uploads/2016/10/IADC-Standard-Manufacturing-Record-Book_V1.0-2016-10-18-FINAL-V2.pdf
- Eng-Tips, "Heat or cast numbers" discussion. eng-tips.com/threads/heat-or-cast-numbers.145119